347H Stainless Steel Pipe

347H Stainless Steel Pipe


1. Standard: ASTM A312 / ASME SA312,ASTM A213/ASME SA213,ASTM A269/ASME SA269
2. Size: 1/2"NB - 16"NB(seamless);1/2"NB - 48"NB (welded)
3. Thickness: 0.5mm-30mm
4. Length: Single, Double Random & Cut Length
5. Grades: Alloy 347h, UNS S34709, WNR.1.4961
Nosūtīt pieprasījumu
Produkta ievads

347H stainless steel pipe is an austenitic stainless steel, including SS 347H seamless pipe, 347H stainless steel welded pipe. A312 347H pipe has a higher carbon content than 347, and has excellent resistance to high temperature oxidation. It is used where intermittent heating between 800ºF (427ºC) and 1650ºF (899ºC) is required. In addition, niobium is added to ASTM A312 GR TP347H material, and niobium and tantalum can refine the grains, giving it excellent resistance to intergranular corrosion.

 

Alloy 347H Tubing Standard:

  • ASTM A312: Standard Specification for Seamless, Welded, and Heavily Cold Worked Austenitic Stainless Steel Pipes

 

  • ASTM A269: Standard Specification for Seamless and Welded Austenitic Stainless Steel Tubing for General Service

 

  • ASTM A213: Standard Specification for Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes

 

 

347h stainless steel pipe

ASTM A312 TP347H Stainless Steel Seamless Pipes Size

6NB - 1200NB
1/8" - 12" NPS
0.6 - 12.7 mm

 

ASTM A312 TP347H Stainless Steel Welded Pipes Size

1/8" - 36" NB, 1/4" - 36" OD
6.35 - 114.3 mm
0.8 - 12.7 mm
up to 26 Meters

 

ASME SA312 UNS S34709 Pipes Specifications

ASTM A312 / ASTM SA 312
ANSI/ASME B36.19M, ANSI/ASME B36.10M
100% X Ray Welded, Seamless, CDW, Fabricated, ERW, Welded
2B, No.4, No.1, No.8 Mirror Finish or custom Finish as per customer Requirements
SCH 5, SCH10, SCH 40, SCH 80, SCH 80S, SCH 160, SCH XXS, SCH XS

 

Chemical Composition of Stainless Steel 347H Pipe

C

P

S

347H

0.04~0.10

Less than or equal to 2.00

Less than or equal to 0.75

17.0~19.0

9.0~13.0

Less than or equal to 0.045

Less than or equal to 0.03

8C~1.00

 

DIN 1.4961 Stainless Steel Pipes Mechanical Properties

Yield   Strength, 0.2% Offset MPa

Elongation   in 2 in. or 51 mm

205

515

40.0

217

 

347H Stainless Steel Pipe Application

 

Why Choose Us AISI 347h Steel Pipe Supplier?

  • EN 10204/3.1B, EN 10204 3.1 and EN 10204 3.2 Material Test Certificate (MTC)

  • Hydrostatic or non-destructive electrical test
  • SGS third-party certification

 

Q: About 347H Stainless Steel Pipe price per kg?

A: Prices ranges from $8 to $15 per kg.

A: Delivery time is within 5-21 days

 

 