Kāds ir Inconel 600 caurules izmērs?
Inconel 600 / UNS N06600 / 2.4816 / Alloy 600 caurulesvārstās no 4 mm līdz 219 mm bezšuvju caurulēm, no 5 līdz 1219,2 mm metinātām un EFW caurulēm ar sieniņu biezumu no 0,5 mm līdz 20 mm. TheLeoy 600 bezšuvju cauruletiek ražots ar aukstās velmēšanas procedūru, un tam ir mazāks absolūtais raupjums un augsta izmēru precizitāte.
Alloy 600 caurules izmēri un izmēri|ANSI B36.10
| DN | NPS | OD(mm) | Sch10 | Sch20 | Sch30 | Sch40 | STS | Sch60 | Sch80 | XS | Sch100 | Sch120 | Sch140 | Sch160 | XXS |
| 6 | 1/8 | 10.3 | 1.24 | 1.45 | 1.73 | 1.73 | 2.41 | 2.41 | |||||||
| 8 | 1/4 | 13.7 | 1.65 | 1.85 | 2.24 | 2.24 | 3.02 | 3.02 | |||||||
| 10 | 3/8 | 17.1 | 1.65 | 1.85 | 2.31 | 2.31 | 3.2 | 3.2 | |||||||
| 15 | 1/2 | 21.3 | 2.11 | 2.41 | 2.77 | 2.77 | 3.73 | 3.73 | 4.78 | 7.47 | |||||
| 20 | 3/4 | 26.7 | 2.11 | 2.41 | 2.87 | 2.87 | 3.91 | 3.91 | 5.56 | 7.82 | |||||
| 25 | 1 | 33.4 | 2.77 | 2.90 | 3.38 | 3.38 | 4.55 | 4.55 | 6.35 | 9.09 | |||||
| 32 | 1 1/4 | 42.2 | 2.77 | 2.97 | 3.56 | 3.56 | 4.85 | 4.85 | 6.35 | 9.7 | |||||
| 40 | 1 1/2 | 48.3 | 2.77 | 3.18 | 3.68 | 3.68 | 5.08 | 5.08 | 7.14 | 10.15 | |||||
| 50 | 2 | 60.3 | 2.77 | 3.18 | 3.91 | 3.91 | 5.54 | 5.54 | 8.74 | 11.07 | |||||
| 65 | 2 1/2 | 73 | 3.05 | 4.78 | 5.16 | 5.16 | 7.01 | 7.01 | 9.53 | 14.02 | |||||
| 80 | 3 | 88.9 | 3.05 | 4.78 | 5.49 | 5.49 | 7.62 | 7.62 | 11.13 | 15.24 | |||||
| 90 | 3 1/2 | 101.6 | 3.05 | 4.78 | 5.74 | 5.74 | 8.08 | 8.08 | |||||||
| 100 | 4 | 114.3 | 3.05 | 4.78 | 6.02 | 6.02 | 8.56 | 8.56 | 11.13 | 13.49 | 17.12 | ||||
| 125 | 5 | 141.3 | 3.40 | 6.55 | 6.55 | 9.53 | 9.53 | 12.7 | 15.88 | 19.05 | |||||
| 150 | 6 | 168.3 | 3.40 | 7.11 | 7.11 | 10.97 | 10.97 | 14.27 | 18.26 | 21.95 | |||||
| 200 | 8 | 219.1 | 3.76 | 6.35 | 7.04 | 8.18 | 8.18 | 10.31 | 12.70 | 12.70 | 15.09 | 18.26 | 20.62 | 23.01 | 22.23 |
| 250 | 10 | 273.1 | 4.19 | 6.35 | 7.8 | 9.27 | 9.27 | 12.7 | 15.09 | 12.70 | 18.26 | 21.44 | 25.4 | 28.58 | 25.40 |
| 300 | 12 | 323.9 | 4.57 | 6.35 | 8.38 | 10.31 | 9.53 | 14.27 | 17.48 | 12.70 | 21.44 | 25.4 | 28.58 | 33.32 | 25.40 |
| 350 | 14 | 355.6 | 6.35 | 7.92 | 9.53 | 11.13 | 9.53 | 15.09 | 19.05 | 12.70 | 23.83 | 27.79 | 31.75 | 35.71 | |
| 400 | 16 | 406.4 | 6.35 | 7.92 | 9.53 | 12.70 | 9.53 | 16.66 | 21.44 | 12.70 | 26.19 | 30.96 | 36.53 | 40.49 | |
| 450 | 18 | 457 | 6.35 | 7.92 | 11.13 | 14.27 | 9.53 | 19.05 | 23.83 | 12.70 | 29.36 | 34.93 | 39.67 | 45.24 | |
| 500 | 20 | 508 | 6.35 | 9.53 | 12.70 | 15.09 | 9.53 | 20.62 | 26.19 | 12.70 | 32.54 | 38.1 | 44.45 | 50.01 | |
| 550 | 22 | 559 | 6.35 | 9.53 | 12.70 | 9.53 | 22.23 | 28.58 | 12.70 | 34.93 | 41.28 | 47.63 | 53.98 | ||
| 600 | 24 | 610 | 6.35 | 9.53 | 14.27 | 17.48 | 9.53 | 24.61 | 30.96 | 12.70 | 38.89 | 46.02 | 52.37 | 59.54 | |
| 650 | 26 | 660 | 7.92 | 12.7 | 9.53 | 12.70 | |||||||||
| 700 | 28 | 711 | 7.92 | 12.7 | 15.88 | 9.53 | 12.70 | ||||||||
| 750 | 30 | 762 | 7.92 | 12.7 | 15.88 | 9.53 | 12.70 | ||||||||
| 800 | 32 | 812.8 | 7.92 | 12.7 | 15.88 | 17.48 | 9.53 | 12.70 | |||||||
| 850 | 34 | 863.6 | 7.92 | 12.7 | 15.88 | 17.48 | 9.53 | 12.70 | |||||||
| 900 | 36 | 914.4 | 7.92 | 12.7 | 15.88 | 19.05 | 9.53 | 12.70 | |||||||
| 38 | 965.2 | 9.53 | 12.70 | ||||||||||||
| 1000 | 40 | 1016 | 9.53 | 12.70 | |||||||||||
| 1050 | 42 | 1066.8 | 9.53 | 12.70 | |||||||||||
| 1100 | 44 | 1117.6 | 9.53 | 12.70 | |||||||||||
| 46 | 1168.4 | 9.53 | 12.70 | ||||||||||||
| 1200 | 48 | 1219.2 | 9.53 | 12.70 |
Īss pārskats par Inconel Alloy 600 caurulēm
Inconel Alloy 600 caurulesparasti ir pieejami plašā izmēru diapazonā, lai tie būtu piemēroti dažādiem rūpnieciskiem lietojumiem. Šīs caurules ir izgatavotas no niķeļa-hroma sakausējuma 600, kas ir pazīstams ar savu lielisko izturību pret koroziju, oksidāciju un augstas temperatūras vidi.
Īpašības: Papildus izturībai pret koroziju un izturībai augstā temperatūrā,2.4816 inconel sakausējums 600piemīt labas mehāniskās īpašības, tostarp augsta stiepes izturība un lieliska metināmība. Šīs īpašības padara to piemērotu lietošanai prasīgās vidēs, kur uzticamība un veiktspēja ir ļoti svarīgas.
Lietojumprogrammas:ASTM B163 / ASME SB 163 Alloy 600 caurulesatrast plašu pielietojumu tādās nozarēs kā ķīmiskā pārstrāde, naftas ķīmija, aviācija, elektroenerģijas ražošana un jūras inženierija. Tos parasti izmanto lietojumos, kuros nepieciešama izturība pret augstām temperatūrām, koroziju un sprieguma korozijas plaisāšanu, piemēram, siltummaiņos, katlos, krāsns komponentos un ķīmiskās apstrādes iekārtās.